PH1310
Polypropylene Homopolymer – MFR: 13 g/10 min*
Apt for injection molding, easily processable, good stability during the process, good stiffness and balance of mechanical properties. Recommended for use in fabricating general parts with a medium wall thickness.
(*) : ASTM D-1238 (2,16kg/230°C)